July 28, 2020

Silver Epoxy Turns Black After an Oxygen Plasma Clean Prior to Wire Bonding…But So What?

Silver Epoxy Turns Black After an Oxygen Plasma Clean Prior to Wire Bonding…But So What? Thomas GreenTJ Green Associates, LLC739 Redfern Lane,Bethlehem, PA 18017email: tgreen@tjgreenllc.com Philipp […]
March 12, 2018

Moisture in Microelectronics: Physics and Chemistry of Volatile Species in Hermetic Electronic Devices

BOOK REVIEW Moisture in Microelectronics: Physics and Chemistry of Volatile Species in Hermetic Electronic Devices By Philipp wh Schuessler I just finished reading this excellent manuscript which […]
October 3, 2017
CMSE Logo

CMSE 2018 Call for Presentations

22nd Annual Components for Military & Space Electronics Conference & Exhibition May 7-10th, 2018 Four Points by Sheraton (LAX) Los Angeles, California Organized by engineers for engineers, […]
September 29, 2017

A Critical Review of MIL-STD-883 Wirebond Visual Inspection Criteria

A Critical Review of MIL-STD-883 Wirebond Visual Inspection Criteria An important consideration in wirebonding is visual inspection of the deformed wire after wirebond formation. The amount […]
June 6, 2017
minnowbrook

Minnowbrook 2017 “Moisture In Microelectronics”

Minnowbrook 2017 “Moisture In Microelectronics” Minnowbrook, A forested retreat at the University of Syracuse Conference Center in the Adirondack Mountains of New York where engineers, scientists […]
October 2, 2016
hermeticity-test-setup

Hermeticity Evaluation Testing

Hermeticity Evaluation Testing Problem Statement: Leak testing per Mil-Std-883 only provides a single, one-time room ambient check of the integrity of the hermetic seal. The reality […]